Specialist equipment is available for carrying out a variety of important tests on asphalt It is important to know how asphalt will react to various conditions such as heat, cold and traffic loads when it is laid on roads. Project specifications will give detailed criteria of what is required, and companies will either ask outside laboratories to make sure the material meets the specs, or will often carry out such tests themselves with trained staff in an on-site laboratory. This will be equipped with the
July 18, 2012 Read time: 5 mins

Specialist equipment is available for carrying out a variety of important tests on asphalt

 It is important to know how asphalt will react to various conditions such as heat, cold and traffic loads when it is laid on roads. Project specifications will give detailed criteria of what is required, and companies will either ask outside laboratories to make sure the material meets the specs, or will often carry out such tests themselves with trained staff in an on-site laboratory.

This will be equipped with the machines capable of carrying out a whole series of tests, and these are done at regular intervals with all the data recorded.

Asphalt is the final product of the refining process of crude oil whose lighter constituents are distilled off to yield gas products such as methane, ethane, propane and butane; naphthas (for processing into gasolines); kerosenes (for processing into jet fuels and light diesels), and gas oils (lubricating oils, and fuel oils). Asphalt is basically crude oil with these lighter products removed.

Asphalts are complex chemical mixtures whose compositions vary widely depending mainly on the source of the crude oil and to a lesser degree, the manufacturing process.

As such, there are numerous tests that can be carried out on them, some are fairly simple and others more complex.


For example, one test among many is the determination of the resistance to hardening under the influences of heat and air and to complete this Italian company 2139 Controls offers its Model 81-B0161/A bitumen oven for the rolling thin-film oven test/RTFOT (EN/European Norm version).

"As is well known, bitumen can be considered as a colloidal system consisting of a mix of high molecular weight hydrocarbons dispersed in minor molecular weight hydrocarbons," says Controls.

By the heat and air action, during mixing, laying and rolling, bitumen loses part of the lighter components, at lower molecular weight, and therefore more volatiles [oils].

"Consequently, the binder is affected by a 'short term ageing' after the mixing and laying work. The bitumen content of the bituminous mixes grants usually a complete cover of aggregates by an average thickness of 9-11 microns on a surface of aggregate mix of the order of 5,000-6,000m²/kg. The high mixing temperature, about 150°C, and the over-heated air affects the binder shared in a very thin film and causes an increase of viscosity and stiffness. The effect is particularly evident at the ambient temperatures." Controls explains that by using the RTFOT apparatus it is possible to perform the loss-on-weight test and to provide the sample 'aged' ready for other tests such as softening point, penetration, dynamic viscosity at 60°C, ductility and other tests in order to verify that the hardening data of bitumen falls within the limits fixed by the specifications for road binders.

According to the US-based 5045 Pioneer Asphalt Company (part of Ziegler Chemical and Mineral Corporation) the softening point and penetration are usually the most commonly used measurements for classifying the properties of asphalts.

Generally, when comparing asphalts, as the softening point increases, the viscosity also increases, the penetration drops and the flash point rises, says the company.

Using various 4814 ASTM (originally the American Society for Testing and Materials) guidelines, the softening point is a range of temperatures that the asphalt softens using a 'ring and ball' technique and is sometimes thought of as the melting point, while penetration (at a prescribed temperature) is how far a weighted needle or cone will sink into the asphalt during a set period of time.

Viscosity (at a prescribed temperature) is an indication of how thick or thin the liquid asphalt is at various temperatures (measured in poises, centipoises (cps), centistokes (cst) or SSU) and the flash point is the temperature that the heated asphalt will flash (ignite briefly).

Indeed, for testing the softening point of asphalts and tar pitches the 81-B0143 Automatic Ring and Ball apparatus is offered by Controls.

The company says the advanced microprocessor-controlled automatic tester is used to determine the softening point of bitumen using, as the heating fluid, water or glycerol.

"The softening point is taken by the interruption of two light barriers suitably positioned, and it can detect the position of the two balls in an independent way.

The temperature is measured by a PT100 sensor placed in a middle position. During operation a magnetic stirrer with adjustable speed assures temperature uniformity in the vessel, and the current temperature and the barriers' status are displayed. The temperature gradient is strictly maintained conforming to the standards throughout the test by the microprocessor control unit.

"The apparatus allows tests to be performed at two different temperature ranges: with boiled or distilled water (the maximum temperature is 80°C) and with glycerol the maximum temperature is 150°C. At the end of the test, the result data are stored in the internal database, or downloaded to a serial printer or to a PC," says Controls.

The company offers its 81-B0100/D and 81-B0101/D Semiautomatic Penetrometers for penetration of bituminous material.

The devices feature a precise digital measurement system as standard, and the 81-B0100/D is the new standard version proposed with the micrometer vertical adjustment and digital measurement of the penetration.

The 81-B0101/D is the new semi-automatic version proposed also with the micrometer vertical adjustment and digital measurement of the penetration and automatic controller for the penetration time.

Both models are provided as standard with the micrometer vertical adjustment fitted in the column base, offering an easier setting of the penetration needle on the sample cup, and a new digital reading of the penetration with 0.01 mm resolution, an exremely accurate reading for a standard penetrometer device.

For more information on companies in this article

Related Content

  • Sophisticated paving technology from BPO
    October 24, 2019
    Advanced technology is enabling asphalt road surfaces to be laid with greater efficiency
  • TRA 2018: pavement additives can stretch a road’s lifespan
    May 9, 2018
    Glass fibre and old tyres can help reduce road wear, according to recent research. Alan Dron reports from the Transport Research Arena – TRA 2018 – event in Vienna. Environmental issues were close to the heart of many presentations at this year’s event at the Reed Exhibition Messe in the Austrian capital from April 16-19. This included decarbonisation – such as making engines more environmentally friendly – and the challenge of digitalisation to create a more efficient transport system.
  • Reducing plant emissions
    February 4, 2025
    Benninghoven offers retrofit solutions to lower emissions from existing asphalt plants.
  • How to maintain a city road by day and Formula 1 track by night
    February 22, 2019
    Nearly a decade on from when Singapore’s Formula 1 (F1) track was first laid, Shell Bitumen’s high-performance binder, Shell Cariphalte, has been selected once more for resurfacing works. The Federation Internationale de l’Automobile (FIA) sets stringent standards for the performance of its tracks, which are made even more challenging given Singapore’s climate. The road surface must remain constant, despite temperatures of up to 30oC and humidity levels above 70%. The 5km Marina Bay Street Circuit, which