An asphalt paving trial at Rome Airport tested mat quality with and without the use of MTVs Rome’s airport Fiumicino or the Leonardo da Vinci Airport of Rome is one of Europe’s busiest airports and lies 25.6km southwest of the city, a 30-minute train ride away.
December 8, 2015 Read time: 4 mins
Local contractor Pavimental used milling machines to remove the old surface of Rome Airport’s runway before bringing in a paving train for resurfacing
RSS

An asphalt paving trial at Rome Airport tested mat quality with and without the use of MTVs

Rome’s airport Fiumicino or the Leonardo da Vinci Airport of Rome is one of Europe’s busiest airports and lies 25.6km southwest of the city, a 30-minute train ride away. Handling just over 38.5 million passengers in 2014, the airport’s three runways carry heavy traffic, so much so that the runway 16L/34R recently required resurfacing. The 3,902m long by 60m wide runway had to be milled and repaved, with local contractor Pavimental winning the contract. The company is considered the leader in asphalt production in Italy.

Before full paving production began on the project, Pavimental wanted to test whether a 1252 Roadtec SB-2500e Shuttle Buggy material transfer vehicle (MTV) could reduce thermal segregation in the hot-mix asphalt (HMA) and ensure a higher-quality finished mat.

The Fiumicino 16L/34R runway project was less than five minutes away from the asphalt plant so the contractor was initially doubtful that MTVs could offer benefits.

The contractor used its 1194 Vögele Super 2100-3i tracked paver for the work, a heavy-duty machine with a maximum laydown rate of 1,100tonnes/hour and a maximum pave width of 13m.

For the three tests conducted, Pavimental had 1228 MOBA as an independent quality controller. MOBA used its PAVE-IR Scan to detect the thermal segregation on the recent paved test layers. The PAVE-IR Scan allows recording of asphalt temperature while paving. It depict a temperature profile and highlights the differences that lead to thermal segregation of the material and identifies areas where premature wear and tear of the road may occur.

Pavimental used the PAVE-IR Scan system to show the overall quality achieved by each paving method. One was paving with the help of the Roadtec SB-2500e/ex Shuttle Buggy MTV. Another was with HMA trucked from the production plant and loaded into the paver.

The determining factor in the research test was to measure the level of thermal segregation occurring in the asphalt mat behind each paving method. In the past, extensive testing resulted in Stroup-Gardiner and Brown establishing in 2000 a classification of thermal segregation and its related consequences. In the classification system, when temperature differences are below 10ºC segregation is considered nonexistent, between 10ºC and 16ºC it is low, between 17ºC and 21ºC medium and it is considered high when over 21ºC.

The higher the measured temperature, the more likely the paved surface will experience fatigue and be less durable. What all the tests point out is that temperature deviations will make pavement less durable and will increase maintenance costs.

For the Rome international airport test, a lift was laid by each method. The testing occurred over a six-day period with test mats laid by each method.

MOBA used infrared scanning to examine the level of thermal segregation. The results concluded that the finished pavement quality from each paving method show a temperature change of <8ºC when using the Roadtec Shuttle Buggy and temperatures varied from between 20ºC and 25ºC when trucked HMA was loaded directly into the paver.

The collected data shows that when the Roadtec Shuttle Buggy is used the maximum thermal segregation detected is 8ºC, so the results indicate NULL segregation, while when the PowerFeeder or direct truck-to-paver methods are used the temperature differentials can be more than 20ºC at any given time. The trucked-in methods will have durability that is expected to be about half of what can be achieved through the Roadtec Shuttle Buggy, which remixes the HMA and provides continuous paving.

Pavimental found the results useful. The initial thinking was that with the HMA production source so close to the jobsite, there would be no need for a material transfer vehicle. However the results of the thermal segregation tests suggest otherwise.

RSS

For more information on companies in this article

Related Content

  • Surface testing
    March 1, 2012
    PipeHawk has used its sophisticated ground probing radar (GPR) technology to develop the e-Spott system for the highways sector. The e-Spott package has been designed and developed in collaboration with another GPR specialist, Utsi Electronics. This new system is said to provide a fast and reliable method of testing the total thickness of bound layers to the sub-base interface or the thickness of surface concrete. This system has advantages over traditional coring methods as there is no need to cause disrup
  • Compaction in the field
    July 31, 2012
    Special applications require stringent quality control and with compaction machines a key part of the paving process, their contribution can be vital. A high quality finish has helped athletes breaking sporting records on the track at the Shanghai Stadium in China during this year's 2008 Summer Olympic Games. Built in 1997 the stadium has been the venue for numerous major sporting events prior to the Olympics, however its track was showing signs of wear and the local authorities decided that a full refurbis
  • The ABG Advantage: What separates these pavers from the competition?
    September 25, 2024
    There are a great many roadbuilding products out there. Sometimes it can be hard to separate the best from the rest.
  • Purdue University creates soybean sealant, Fluid iSoylator, for concrete
    October 9, 2015
    Researchers at Purdue University in the United States have developed a hydrophobic sealant that could prevent potentially damaging fluids from entering concrete pores. Paul Imbrock, founder and president of Environmental Concrete Products – the university’s spin-off company - said the firm’s Fluid iSoylator product can be used to protect new and existing concrete. "Our product is absorbed into dry concrete's pore network to create a hydrophobic barrier that prevents potentially damaging fluids from en